Juran Noh
Yangang Liang
2025_JuranNoh_YangangLiang_ACS.Appl.Energy.Mater._5c02546 ← click to see all uploads from this cell
2026-08-14 18:21:42
65326c39-3a8a-4fb4-8c60-86a592de4791
How to Cite
1 — Cite the dataset paper
↗ View paper
2 — Cite the ESRA platform
Galib, M. et al. (2026). ESRA: Energy Storage Research Assistant. Argonne National Laboratory. https://github.com/MusannaGalib/esra-platform
CC BY 4.0  ·  Data shared under Creative Commons Attribution 4.0

Storage LocationNERSC Community File System

/global/cfs/cdirs/m4845/gsharing/yangang-liang/automation-accelerated-electrolyte-desig/2025-jurannoh-yangangliang-acsapplenergy/2025_JuranNoh_YangangLiang_ACS.Appl.Energy.Mater._5c02546/eis/ESRA-EIS-0012/
Open in Globus File Manager →

Linked Uploads

Type Group Date Project Link
NMR Yangang Liang 2026-08-14 18:21 Automation-Accelerated Electrolyte Design Mitigates Solubility Competition between Redox-Active Molecules and Supporting Salts same cell
MLIP Yangang Liang 2026-08-14 18:21 Automation-Accelerated Electrolyte Design Mitigates Solubility Competition between Redox-Active Molecules and Supporting Salts same cell
DFT Yangang Liang 2026-08-14 18:21 Automation-Accelerated Electrolyte Design Mitigates Solubility Competition between Redox-Active Molecules and Supporting Salts same cell

Materials Studied 3 materials

Material Family Role(s) Ion
2,1,3-benzothiadiazole (BTZ)  · BTZ redox-active organic molecule
~3 M ROM in the non-aqueous redox-flow electrolyte
Redox-active organic
Other
Redox-active species Li
LiTFSI  · Lithium bis(trifluoromethanesulfonyl)imide Lithium imide salt
Other · as named
Salt Li
m-xylene / acetonitrile mixed solvent  · MX/ACN solvent blend
MX/ACN about 0.3/0.7 v/v; ~5 mS/cm
Aromatic-nitrile mixed solvent
Liquid · as named
Electrolyte, Solvent Li

Declared for sample 2025_JuranNoh_YangangLiang_ACS.Appl.Energy.Mater._5c02546 — shared by every dataset on this sample.

Experiment Metadata

Visibility public
Temperature C 24.0
Publication Doi 10.1021/acsaem.5c02546
Institution Code ESRA
Electrode Area Cm2 4.0